Product Details:
Payment & Shipping Terms:
|
Purity: | 99.95%(3N5)min | Size: | 3-10mm |
---|---|---|---|
Application: | Additive For Special Alloy | Packing: | In Drums |
Material: | Nb1, Nb2 | Standard: | ASTM B 391 |
High Light: | niobium crucible,niobium ring |
Additive Niobium Metal Purity 99.95%min For Superalloy Size 3-10mm Small Pieces
Application: high purity niobium metals are ainly used as additives to niobium-base alloys, high strength low alloy steel and stainless steel for oil and gas pipelines, superalloy, superconducting materials and high-temperature alloys. It is also the raw material of electronic beam melted niobium ingot.
Properties: high purity, high temperature resistance, good anti-corrosion, low oxygen, low carbon, low impurities, suitable for superalloy additive.
Specification: 3-10mm, other sizes of niobium metals are available upon requests.
Packing: inplastic bags in drums,
Purity: 99.95%min(3N5min)
Impurities
Metallic impurities, ppm max by weight, balance: Niobium
Element | Zr | Ta | Fe | Si | W | Ni | Mo | Hf |
Content | 200 | 1000 | 50 | 50 | 300 | 50 | 100 | 200 |
Non-Metallic impurities, ppm max by weight
Element | C | N | O | H |
Content | 100 | 100 | 150 | 15 |
The EB furnace technology smelted niobium Ingots can be forged and rolled and then cut into 3-10mm small pieces. The size can be customized as per requests of the clients.