Home
Products
About Us
Factory Tour
Quality Control
Contact Us
Request A Quote
News
Baoji Towin Rare Metals Co.,Ltd
Home ProductsNiobium Ingot

3N5-4N Niobium Ingots for Special Steel Additive and Superalloy Material

China Baoji Towin Rare Metals Co.,Ltd certification
We appreciate your nice services and the perfect sputtering targets Towin supplied. We would like to enter into a long term cooperation with Towin Rare Metals.

—— Simon

Reliable factory providing excellent products and services. The specification and quality exceeds ourexpects. Very good, thanks!

—— Bruno Pascal

Very professional team and advanced equipment. Your price is beautiful and the products are perfect. The performance of niobium sheets and plates performs quite well !

—— James Daniel

I'm Online Chat Now

3N5-4N Niobium Ingots for Special Steel Additive and Superalloy Material

3N5-4N Niobium Ingots for Special Steel Additive and Superalloy Material
3N5-4N Niobium Ingots for Special Steel Additive and Superalloy Material

Large Image :  3N5-4N Niobium Ingots for Special Steel Additive and Superalloy Material

Product Details:
Place of Origin: CHINA
Brand Name: TOWIN
Certification: ISO9001
Model Number: RO4200, RO4210
Payment & Shipping Terms:
Minimum Order Quantity: Negotiable
Price: Negotiable
Packaging Details: Wooden Box
Delivery Time: 2-3days
Payment Terms: T/T
Supply Ability: 10MT tons per month
Detailed Product Description
Material: Nb1, Nb2 Purity: 99.95%-99.99%
Technology: EB Furnaced Smelted Standard: ASTM B391
Diameter: 300max Shape: Ingot
High Light:

sheet ingot

,

ingot casting

3N5-4N Niobium Ingots for Special Steel Additive and Superalloy Material

 

Niobium ingot is  soft, grey, crystalline, ductile transition metal which is used in various superconducting materials. Its melting point is 2468℃ and boiling point 4742℃. It has the characteristics of high temperature resistance, high corrosion resistance and good ductility. Therefore, niobium ingots are widely used in electronics, iron and steel industry, chemical, jewelry, superconducting, engineering, aviation, aerospace industry etc.

 

Grade: RO4200, RO4210
Purity:99.95%(3N5)
Manufacturing Standard: ASTM B 391-96

Diameter: φ300mm, φ210mm, φ150mm (Other diameter available upon requests)

 

 

Specifications

Metallic impurities, ppm max by weight, balance: Niobium (Other specification can be required)

Element Zr Ta Fe Si W Ni Mo Hf
Content 200 1000 50 50 300 50 100 200


Non-Metallic impurities, ppm max by weight

Element C N O H
Content 100 100 150 15

 

Diameter can be choosed such as: Φ295×L,Φ215×L,Φ145×L