Product Details:
Payment & Shipping Terms:
|
Manufacturing Standard: | ASTM B392-99 | Recrystallization: | 95%min |
---|---|---|---|
Property: | Heat-resistant, Corrosion Resistant, Good Ductility | Boiling Point: | 4742 ℃ |
Melting Point: | 2468 ℃ | Density: | 8.57 G/cm3 |
Delivery Time: | 2-3weeks | Surface: | Polished |
High Light: | niobium bar,nb wire |
ASTM B392-99 Niobium Rods, 99.99% (4N) Purity , Rods of EB Furnace Smelted Niobium Metal
Our Strength
Application: Niobium mechanical parts, electric materials, high voltage sodiumlamp
Grade:RO4200,RO4210
Purity: 99.95%(3N5)-99.99%(4N)
Manufacturing Standard: ASTM B392-99
Specifications
Metallic impurities, ppm max by weight, Balance - Niobium
Element | Fe | Mo | Ta | Ni | Si | W | Zr | Hf |
Content | 50 | 100 | 1000 | 50 | 50 | 300 | 200 | 200 |
Non-Metallic impurities, ppm max by weight
Element | C | H | O | N |
Content | 100 | 15 | 150 | 100 |
Mechanical properties for annealed rods 0.125in(3.13mm)-2.5in(63.5mm)
Ultimate Tensile Strength (MPa) | 125 |
Yield strength (MPa, 2% offeset) | 73 |
Elongation(%, 1-in gage length) | 25 |
Dimensional Tolerance for Rods and Wires
Diameter in (mm) | Tolerance in (±mm) |
0.020-0.030(0.51-0.76) | 0.00075(0.019) |
0.030-0.060(0.76-1.52) | 0.001(0.025) |
0.060-0.090(1.52-2.29) | 0.0015(0.038) |
0.090-0.125(2.29-3.18) | 0.002(0.051) |
0.125-0.187(3.18-4.75) | 0.003(0.076) |
0.187-0.375(4.75-9.53) | 0.004(0.102) |
0.375-0.500(9.53-12.7) | 0.005(0.127) |
0500-0.625(12.7-15.9) | 0.007(0.178) |
0.625-0.750 (15.9-19.1) | 0.008(0.203) |
0.750-1.000 (19.1-25.4) | 0.010(0.254) |
1.000-1.500 (25.4-38.1) | 0.015(0.381) |
1.500-2.000 (38.1-50.8) | 0.020(0.508) |
2.000-2.500 (50.8-63.5) | 0.030(0.762) |